Gold - Gneiss
Quarry Location: Pirin Mountains range in southwestern Bulgaria
Water Absorption: 0.52 %
Density: 2600 kg/m3
Flexural Strength: 15 -17 MPa
Compressive Strength: 55 - 65 MPa
Recommended Usage: building stone, monuments, pool coping, sills, ornamental stone, interior, exterior, wall, floor, paving
Finishing Surface: Bush Hammered,Tumbled,Brushed,Honed,Split,Machine Cut,Natural Surface,Sandblasted,Combed,Filled,Chiseled,Pickling
Additional Names: Arda Quartzite, Arda Gold Gneiss, Arda Golden Gneiss,Sofia Gold Gneiss,Sofia Yellow Gneiss, Gloria-Gneiss,Gneis Gloria,Gneiss Gloria Yellow Gneiss,Arda Golden Beige Gneiss,Gneiss Gold Quartzite,Popsko Gold Gneiss,Gold Gneiss,Pirin Gold Gneiss