acrylic, polyurethane sealant, epoxy sealants, Stone adhesives, abrasives, waxes, Sealers and impregnators
acrylic, polyurethane sealant, epoxy sealants, Stone adhesives, abrasives, waxes, Sealers and impregnators
COMPOSITION COMPONENT A: Thixotropized pure epoxy resin (molecular weight <700) COMPONENT B: Mix of adducts of cycloaliphatic amines, polyamides and tertiary amines, thixotropized, with fillers and pigments USE Permanent gluing of marbles, naatural stones to each other or to other materials (metals, concrete, terracotta etc.). For interior and exterior.
COLOUR Transparent opaque
MIXING RATIO
Epoxy adhesives require exact mixing ratio, in weight, between component A (resin) and component B (catalyst). In
this particular case the ratio is:
COMPONENT A : COMPONENT B = 100 : 100
(i.e.: 100 gr. of component A mixed with 100 gr. of component B)
PACKAGING
EPOXY TOP component A 0.4oo kg. metal tin
EPOXY TOP component B 0.4oo kg. metal tin
SURFACE PREPARATION Surfaces to be treated/glued to be porous, clean, dry and free from dust, grease or any other extraneous substances
MIXING Mix the quantities as indicated in
MIXING RATIO section until to obtain an homogeneous texture
APPLICATION With putty knife or by spreading. Do not apply at temperature lower than +10°C (50°F) Suggested temperature of application +10°C (50°F) and +30°C (86°F)
THICKNESS The best adhesive characteristics are obtained with thicknesses of adhesive from 0.3 to 1.0 mm
CONSUMPTION 250 to 700 g/m²
POLYMERISATION The rate of reaction increases with the temperature, which should never be lower than +10°C (50°F).
HARDENING at 25°C (77°F) 15 minutes in mass, 25 minutes in thin coat (applied).
NOTE Based on the data reported, workability time is considered to be 5 to10 minutes Do not store at temperature lower than 5°C (41°F) and higher than 35°C (95°F) Protect from frost the stored cans/tins.