The composition of onyx
Compressive strength of the dry stone: Sa 109.10 MPa
Soaked compressive strength of stone: Sat 104.80 MPa
Compressive strength after freezing and thawing (25 cycles): So 83.20 MPa
Water Absorption: σ 2.3
Bulk density: γ 2685 kg/m3
Wear resistance: 20.3 cm2 cm3/50